Phenolic epoxy resin is made by the reaction of linear phenolic resin and epichlorohydrin in the presence of NaOH. Commonly used phenolic epoxy resins are PNE type phenolic epoxy resin, BNE type phenolic epoxy resin, CNE type phenolic epoxy resin. Phenolic epoxy resins are widely used in the fields of machinery and electronics, aerospace, transport, construction and so on because of their excellent process performance, mechanical properties and physical properties.
											  
											  												  