Divinyl ether YLD-S0101 is a diethylene glycol divinyl ether, CAS 764-99-8, that cures by cationic polymerization, not by amine addition. The product page states purity min. 99.0 %, APHA max. 50 and water max. 0.5 %; the companion grade YLD-S0102, CAS 765-12-8, is the triethylene glycol homologue.
A glycidyl ether carries an epoxide ring that opens by nucleophilic addition, so its dosage follows AHEW and EEW. A divinyl ether carries an electron-rich double bond that polymerizes under a cation, typically a sulfonium salt activated by ultraviolet light.
The two react by different routes and are not interchangeable in a stoichiometric calculation. No phr figure can therefore be derived from 100 × AHEW ÷ EEW. A vinyl ether diluent is dosed by initiator level and viscosity target instead.
Table 1. Values as published on the two product pages. The boiling point row carries no pressure reference on the page, so it should not be read as an atmospheric figure.
| Item | YLD-S0101 | YLD-S0102 |
| Chemical name | Diethylene glycol divinyl ether | Triethylene glycol divinyl ether |
| CAS No. | 764-99-8 | 765-12-8 |
| Appearance | Colorless transparent liquid | Colorless or light yellow liquid |
| Assay, % | Purity min. 99.0 | DVE-3 content min. 98.0 |
| Color, APHA | max. 50 | not stated |
| Water, % | max. 0.5 | max. 0.20 |
| Density, g/mL at 25 °C | not stated | 0.99 |
| Boiling point, °C | not stated | 120–126 |
From the molecular formulas, the vinyl equivalent weight calculates to 79.1 g per vinyl group for C8H14O3 at 158.19 g/mol, against 101.1 g/eq for C10H18O4 at 202.25 g/mol. Both figures are calculated, not measured, and should be confirmed against our TDS.
A divinyl ether enters a UV-cationic coating as the reactive fraction, typically 10–30 phr against an epoxy or oxetane base, with a triarylsulfonium photoinitiator at 1–3 phr. Neither product page publishes a recommended loading, so these are application ranges.
Table 2. Starting points for a formulation trial, separated by basis; only the equivalent weights are derived from published data.
| Parameter | Starting range | Basis |
| Vinyl ether fraction | 10–30 phr | application range, not published |
| Photoinitiator | 1–3 phr | application range, not published |
| Vinyl equivalent weight, YLD-S0101 | 79.1 g/eq | calculated from C8H14O3 |
| Vinyl equivalent weight, YLD-S0102 | 101.1 g/eq | calculated from C10H18O4 |
YLD-S0101 carries the higher vinyl density at 79.1 g/eq and is the faster of the pair. YLD-S0102 states DVE-3 content min. 98.0 % and density 0.99 g/mL at 25 °C, and its longer glycol chain gives the more flexible network.
Neither page publishes viscosity, so a dilution level should be fixed against the TDS rather than against a catalogue figure. For a first trial, request 500 g of YLD-S0101 and run it against the same loading of YLD-S0102 in the intended coating. Compare gel time at equal photoinitiator level, then check adhesion once the film has cured. The coatings application note sets out the film requirements the pair has to meet.