YLD-S0102, chemical name Triethylene Glycol Divinyl Ether, CAS No. 765-12-8.

YLD-S0102 is a colorless to pale yellow liquid with low volatility. It is an organic compound that is soluble in water and common organic solvents. Triethylene glycol divinyl ether is often used as an industrial solvent in the fields of fibers, resins, coatings, spray paints and adhesives. It is a reactive diluent for UV and peroxide curing adhesives and sealants. It is also a component of sulfur-based sealant compounds. It can be used as a crosslinker in the production of polyacrylate ion exchange resins.

 

 

 

Item

Specification 

Appearance

Colorless or light yellow liquid

DVE-3 Content, %

Min. 98.0

Boiling Point, °C

120-126

Density, g/mL @25°C

0.99

Moisture Content, %

Max. 0.20

 

  • Gel-Free Cationic Polymerization: Enables complete conversion (up to 100%) without gelation, ensuring predictable and controlled network formation—a unique advantage over conventional divinyl ethers.
  • Exceptional Reactivity: Achieves rapid cure with low shrinkage and high double-bond conversion in photoinitiated cationic and dual-cure systems.
  • Superior Hydrogel Performance: Produces larger gel fractions and more homogeneous networks compared to conventional crosslinkers (e.g., MBA), with excellent mechanical properties.
  • Dual-Cure Versatility: Compatible with both cationic and free-radical polymerization mechanisms.

 

  • Advanced Polymer Synthesis: Comonomer and crosslinking agent for specialty polymers, including polyacrylate ion exchange resins and polyvinyl ether copolymers.

  • Hydrogels & Biomedical Materials: Crosslinker for hydrogels used in drug delivery, tissue engineering, and water purification; low toxicity makes it preferable to alternatives like MBA..

  • Lithium-Ion Batteries: Component in gel polymer electrolytes, improving ionic conductivity and mechanical integrity.

  • Polymer Modification: Modifier to enhance hydrophilicity, flexibility, toughness, and processability in coatings, finishes, and lubricant additives.

 

Storage in a cool and dry place, Avoid direct sunlight. All safety information is provided in the Material Safety Data Sheet.

 

12 months from the date of manufacture in the original packing in ambient temperatures.

 

Drums.

 

leave a message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.
Hot Products

Related Products

Diluent sample
Triethylene Glycol Divinyl Ether YLD-S0102

YLD-S0102, chemical name Triethylene Glycol Divinyl Ether, CAS No. 765-12-8.

Diluent sample
Diethylene Glycol Divinyl Ether YLD-S0101

YLD-S0101, chemical name Diethylene Glycol Divinyl Ether, CAS No. 764-99-8.

Diluent sample
High-Flexibility Cardanol Diglycidyl Ether YLD-9016

YLD-9016, chemical name Cardanol Diglycidyl Ether, CAS No. 68390-54-5.

Diluent sample
Low-Viscosity Enhanced Cardanol Diglycidyl Ether YLD-9014A

YLD-9014A, chemical name Cardanol Diglycidyl Ether, CAS No. 68390-54-5.

Diluent sample
General-Purpose Standard Cardanol Diglycidyl Ether YLD-9014

YLD-9014, chemical name Cardanol Diglycidyl Ether, CAS No. 68390-54-5.

Diluent sample
Diethylene glycol diglycidyl ether YLD-2003

YLD-2003, chemical name Diethylene glycol diglycidyl ether, CAS No. 39443-66-8.

Diluent sample
Polypropylenglycol diglycidyl ether YLD-2005

YLD-2005, chemical name Polypropylenglycol diglycidyl ether, CAS No. 26142-30-3.

Diluent sample
2-Methylphenyl Glycidyl ether YLD-6002

YLD-6002, chemical name 2-Methylphenyl Glycidyl ether, CAS No. 2210-79-9.

Diluent sample
4-tert-Butylphenyl glycidyl ether YLD-6004

YLD-6004, chemical name 4-tert-Butylphenyl glycidyl ether, CAS No. 3101-60-8.

Diluent sample
(C8-10)alkylglycidyl ether YLD-7004

YLD-7004, chemical name (C8-10)alkylglycidyl ether, CAS No. 68609-96-1.

Diluent sample
Allyl glycidyl ether YLD-9005

YLD-9005, chemical name Allyl glycidyl ether, CAS No.106-92-3. 

Diluent sample
Tetrahydrophthalic acid diglycidylester YLD-9012

YLD-9012, chemical name Tetrahydrophthalic acid diglycidylester, CAS No. 21544-03-6.

Diluent sample
N N-DIGLYCIDYLANILINE YLD-9013

YLD-9013, chemical name N,N-Diglycidylphenylamine, CAS No. 2095-06-9.

Diluent sample
Cardanol glycidyl ethers YLD-9006

YLD-9006, chemical name Cardanol glycidyl ethers, CAS No. 171263-25-5.

Diluent sample
Butyl glycidyl ether(BGE) YLD-9004

YLD-9004, chemical name Butyl glycidyl ether(BGE), CAS No. 2426-08-6. 

Diluent sample
Neopentyl glycol diglycidyl ether YLD-6009

YLD-6009, chemical name Neopentyl glycol diglycidyl ether, CAS No. 17557-23-2.

Diluent sample
1,4-Butanediol diglycidyl ether YLD-6018L

YLD-6018L, chemical name 1,4-Butanediol diglycidyl ether, CAS No. 2425-79-8.

Diluent sample
1,6-Hexanediol diglycidyl ether YLD-6008

YLD-6008, chemical name 1,6-Hexanediol diglycidyl ether, CAS No. 16096-31-4. 

Diluent sample
Benzyl glycidyl ether YLD-6021

YLD-6021, chemical name Benzyl glycidyl ether, CAS No. 89616-40-0.

Diluent sample
Glycidyl phenyl ether YLD-6001

YLD-6001, chemical name Glycidyl phenyl ether, CAS No. 122-60-1. 

Diluent sample
Castor oil glycidyl ether YLD-9003

YLD-9003, chemical name Castor oil glycidyl ether, CAS No. 74398-71-3. 

Diluent sample
1,2,3-Propanetriol glycidyl ether YLD-6011

YLD-6011, chemical name 1,2,3-Propanetriol glycidyl ether, CAS No. 13236-02-7.

Diluent sample
Pentaerythritol glycidyl ether YLD-6013

YLD-6013, chemical name Pentaerythritol glycidyl ether, CAS No. 3126-63-4. 

Diluent sample
Resorcinol diglycidyl ether YLD-6010

YLD-6010, chemical name Resorcinol diglycidyl ether, CAS No. 101-90-6. 

Diluent sample
Trimethylolpropane triglycidyl ether YLD-6012

YLD-6012, chemical name Trimethylolpropane triglycidyl ether, CAS No. 30499-70-8. 

Diluent sample
Neodecanoic acid glycidyl ester YLD-8001

YLD-8001, chemical name Neodecanoic acid glycidyl ester, CAS No. 26761-45-5. 

Diluent sample
Alkyl (C12-C14) glycidyl ether YLD-7003

YLD-7003, chemical name Alkyl (C12-C14) glycidyl ether, CAS No. 68609-97-2. 

Diluent sample
Hexahydro-phthalic acid diglycidylester YLD-8003

YLD-8003, chemical name Hexahydro-phthalic acid diglycidylester, CAS No. 5493-45-8. 

leave a message

leave a message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.
submit

home

products

WhatsApp

Contact Us