Non-crystalline epoxy resin is a liquid bisphenol A grade whose EEW band is widened to 185-220 g/eq in YLE-128R and 205-240 g/eq in YLE-128S. A wider band slows the lattice that clouds standard resin near 5 °C, and viscosity reaches 25,000 mPa·s. Phr moves 16% across the band, so dosing is per drum.

Figure 1. Clear liquid bisphenol A epoxy resin beside a condensate-covered drum lid: clarity at low temperature is the property under test.
The complaint rarely starts in a laboratory. It starts in a shed that fell to 2 °C overnight, or in a container that crossed a mountain pass in January.
A standard liquid bisphenol A resin leaves the plant water-clear at 25 °C and arrives hazy, with grit in the drum head.
Standard liquid bisphenol A epoxy resin such as YLE-128 sits at 184-190 g/eq on the same product page, about 0.10 to 0.14 repeat units per molecule. That band is narrow enough to pack, and one nucleus seeds the rest.
YLE-128R and YLE-128S widen the band to 185-220 and 205-240 g/eq. This report separates symptom from cause, then prices the trade-off in phr.
Both grades are bisphenol A diglycidyl ether. The backbone does not change; only the EEW distribution and the viscosity band move.
Table 1 collects what Yolatech publishes. YLE-128R and YLE-128S share the bisphenol A epoxy resin product page with YLE-127, YLE-128 and YLE-130.
Table 1. Product identification for YLE-128R and YLE-128S, from the bisphenol A epoxy resin product page and the 2026 catalog, page 3.
Item |
Information |
Chemical name |
Bisphenol A diglycidyl ether |
Appearance |
Clear pale liquid, color max. 1 Gardner |
EEW |
185-220 g/eq / 205-240 g/eq |
Viscosity at 25 °C |
11,000-25,000 mPa·s / 12,000-25,000 mPa·s |
Hydrolyzable chlorine |
printed as 2% for YLE-128R / 5,000 ppm for YLE-128S |
Catalog application |
Composite, adhesives, coating, flooring |
CAS number |
not printed on the page, confirm on the COA |
Table 2 places both grades beside YLE-128, the grade they replace. The EEW span row carries the argument.
Table 2. Property comparison of YLE-128R, standard YLE-128 and YLE-128S.
Property |
YLE-128R |
YLE-128 |
YLE-128S |
EEW, g/eq |
185-220 |
184-190 |
205-240 |
EEW span, g/eq |
35 |
6 |
35 |
Viscosity at 25 °C, mPa·s |
11,000-25,000 |
11,000-15,000 |
12,000-25,000 |
Color as printed |
1 Gardner |
50 APHA |
1 Gardner |
Hydrolyzable chlorine |
2% as printed |
500 ppm |
5,000 ppm |
EEW is determined by titration according to ASTM D1652, with ISO 3001 as an equivalent route. Viscosity is quoted at 25 °C, and color follows ASTM D1544.
No wet-lab work was performed. Each physical value is a page or catalog figure, and each phr value is calculated. Water content, if it matters, follows ASTM E203.
Crystallization needs order, and order needs a narrow distribution. Widen the distribution and the melting range drops.
For a bisphenol A diglycidyl ether oligomer, EEW follows 170 + 142n, where n is the average repeat count. EEW 185 gives n = 0.11 and EEW 220 gives n = 0.35.
That spread is the mechanism. Mixed homologues cannot stack on one lattice, the melting range broadens downward, and the driving force for nucleation shrinks.
Nucleation is slowed, not removed. A seeded drum held at 0 °C still clouds.
Viscosity is the price. YLE-128R reaches 25,000 mPa·s against 15,000 mPa·s, a 67% higher ceiling, because higher oligomers carry more mass.
Reactivity moves the other way. EEW 220 needs 82.7 phr of YLH-3002 where EEW 185 needs 98.4 phr, so one drum can shift the mix ratio by 16%.
Table 3 sets YLE-128R against the standard grade and liquid bisphenol F, the usual low-viscosity answer.
Table 3. YLE-128R against two alternatives on the properties that decide cold-storage behaviour.
Property |
YLE-128R |
YLE-128 |
YLE-170 (liquid BPF) |
EEW, g/eq |
185-220 |
184-190 |
160-180 |
Viscosity at 25 °C, mPa·s |
11,000-25,000 |
11,000-15,000 |
2,000-5,000 |
Color as printed |
1 Gardner |
50 APHA |
max. 1 Gardner |
Hydrolyzable chlorine |
2% as printed |
500 ppm |
500 ppm |
Crystallization risk in cold storage |
reduced by band width |
high |
high on low-chloride grades |
Effect on mixed viscosity |
higher than standard |
baseline |
much lower |
Bisphenol F buys flow, 2,000-5,000 mPa·s against 11,000-25,000 mPa·s, but the catalog labels its low-chloride grades crystalline epoxy resin, so cold storage still bites. If flow outranks clarity, liquid bisphenol F resin wins; if clarity outranks flow, it does not.
Hardener mass follows phr = 100 × AHEW ÷ EEW, with AHEW from the hardener data sheet and EEW from the resin lot.
Table 4 runs the formula at the mid-point of each band for three hardeners.
Table 4. Hardener demand in phr, calculated from AHEW and the mid-point EEW of each band.
Hardener (AHEW, g/eq) |
YLE-128 at EEW 187 |
YLE-128R at EEW 202.5 |
YLE-128S at EEW 222.5 |
YLH-3002 (182) |
97.3 phr |
89.9 phr |
81.8 phr |
YLH-5022 (175) |
93.6 phr |
86.4 phr |
78.7 phr |
YLH-6005 (95) |
50.8 phr |
46.9 phr |
42.7 phr |
YLH-3002, whole band |
95.8-98.9 phr |
82.7-98.4 phr |
75.8-88.8 phr |
Read the bottom row before ordering. YLE-128R carries 15.7 phr of movement inside one band.
Dose at 89.9 phr and a 220 g/eq lot arrives with 8.7% excess amine; the network plasticizes and a damp wall blushes. A 185 g/eq lot leaves the same mix 8.6% short.
Titrate each lot. A phr copied from the last drum is an assumption, not a specification.
Heat fixes the symptom if the drum is warmed evenly and stirred before sampling.
• Warm to 45-50 °C, not 70 °C. Above 60 °C the color drifts and the drum skin scorches.
• Roll or stir the whole drum. Clear liquid decanted off a crystalline heel carries seeds forward.
• Hold the mixed system above 15 °C. Below that, YLE-128S tops out near 25,000 mPa·s and air stops rising.
• Filter if grit shows. A 200 µm screen catches the crust without stripping resin.
Table 5. Field symptoms, their causes, and the action that clears them.
Symptom |
Likely cause |
Action |
haze at 5 °C, clear at 25 °C |
incipient crystallization |
warm to 50 °C, stir, retest |
grit in the drum head |
settled crystals |
roll the drum, do not decant |
solid ring on the wall |
nucleation at a cold wall |
melt the ring, homogenise |
viscosity above 25,000 mPa·s |
cold resin, not a spec shift |
recheck at 25 °C first |
blush on a damp wall |
amine excess from a low-EEW lot |
retitrate EEW, recalculate phr |

Figure 2. A drum opened after cold storage: the surface skin is melted and homogenised before any sample is taken.
Four application areas take most of the volume, each failing differently.
Flooring sets the hardest viscosity demand: self-levelling needs flow at 15 °C, and the 25,000 mPa·s ceiling leaves little room.
Dose 89.9 phr of YLH-3002 at EEW 202.5. The failure mode is a cold pour that will not close a trowel mark.
Wet lay-up runs YLE-128R at 89.9 phr with YLH-3002 or 86.4 phr with YLH-5022 polyamide hardener, depending on pot life.
Risk sits in a batch warmed only at the wall: the lay-up cures unevenly and shows white streaks.
Adhesives want the higher-EEW end, where YLE-128S at 222.5 g/eq gives 81.8 phr with YLH-3002 modified cycloaliphatic amine and a longer open time.
The 5,000 ppm chlorine level rules YLE-128S out of electronic bonds; construction adhesives do not care.
Coatings accept the viscosity and gain cold-weather clarity; haze shows in a gloss finish.
Pair with YLH-5022 at 86.4 phr for flexibility, or YLH-6005 at 46.9 phr where a 5 °C cure matters more than pot life.
Table 6. Application, dose and failure point for the two grades.
Application |
Dose |
Function |
Failure point |
cold-climate flooring |
89.9 phr YLH-3002 |
flow at 15 °C |
cold pour that will not level |
wet lay-up composite |
86.4 phr YLH-5022 |
wet-out at workable viscosity |
uneven cure after partial remelt |
structural adhesive |
81.8 phr YLH-3002 on YLE-128S |
longer open time |
amine excess on a low-EEW lot |
protective coating |
86.4 phr YLH-5022 |
gloss and clarity |
haze from a crystalline heel |
winter primer |
46.9 phr YLH-6005 |
fast set at 5 °C |
short pot life in a warm shop |

Figure 3. Clear resin drawn across a glass laminate: haze from a crystalline heel shows as white streaks under the surface.
Two limits are hard. YLE-128S carries 5,000 ppm hydrolyzable chlorine, which puts it outside electronic potting; the low-chloride 128K, 128L and 128P grades cover that work.
A widened band suppresses crystallization, it does not abolish it. Weeks below 0 °C still produce nuclei.
Stoichiometry is the quieter limit. EEW 185-220 spans 19%, so one phr fits one lot and misses the next.
One chlorine figure needs care. The product page and the catalog both print 2% for YLE-128R, which does not match the ppm scale used on the same row, so treat it as unverified until a COA confirms it.
A second discrepancy concerns YLE-128. The catalog prints 184-194 g/eq against 184-190 on the page, so this report uses the page value; a COA settles it.
Verify EEW on every lot according to ASTM D1652, and hold a retained sample at 5 °C for seven days to watch for haze.
Storage above 15 °C avoids most incidents; a heated room costs less than a returned drum. Read the current TDS, MSDS and COA before reformulating.
• Check the drum head on receipt. A crust means the drum crossed a cold leg.
• Do not stand IBCs on a concrete floor in an unheated shed; the base is the coldest point.
• Keep uncured resin off skin. Bisphenol A epoxy is a sensitiser; gloves are the control.
Standard liquid bisphenol A resin starts to crystallize near 0-10 °C, fastest a few degrees below its melting range. YLE-128R widens that window, and does not close it.
No. Both are bisphenol A diglycidyl ether. YLE-128R carries a wider oligomer distribution, EEW 185-220 g/eq against 184-190 g/eq, and that distribution is the product.
Yes, by warming to 45-50 °C and rolling until the ring and the heel are gone. Decanting the clear top layer leaves the seeds behind and the batch clouds again within days.
YLE-128R. At EEW 202.5 g/eq it takes 89.9 phr of YLH-3002, while YLE-128S at 222.5 g/eq takes 81.8 phr, a 10% difference in hardener mass.
Slightly. Higher oligomer content lowers epoxy content per kilogram, so a 185 g/eq lot cures harder than a 220 g/eq lot of the same grade.
No. At 5,000 ppm hydrolyzable chlorine it is a general-purpose grade. The 128K, 128L and 128P grades are the low-chloride options for potting.
YLE-128R and YLE-128S hold clarity through cold freight by widening the EEW band to 185-220 and 205-240 g/eq. The cost is a 25,000 mPa·s ceiling and a phr that moves 16% across the band.
Dosing from one fixed phr is the failure that follows. Titrate each lot, warm the drum evenly, and stir before sampling.
Where flow outranks clarity, liquid bisphenol F remains the better trade.
Yolatech product page, bisphenol A epoxy resin: https://www.yolatech.com/bisphenol-a-epoxy-resin (accessed 2026-11-30).
Yolatech Technical Data Sheet for YLE-128R and YLE-128S, bisphenol A diglycidyl ether (available on request).
Yolatech Certificate of Analysis (COA) for YLE-128R, bisphenol A diglycidyl ether (available on request).
ASTM D1652, epoxy content of epoxy resins (EEW).
ISO 3001, determination of epoxy equivalent.
ASTM D1544, Gardner color of transparent liquids.
ASTM E203, water content by Karl Fischer titration.