Polypropylenglycol diglycidyl ether YLD-2005

YLD-2005, chemical name Polypropylenglycol diglycidyl ether, CAS No. 26142-30-3.

YLD-2005 is low total chlorine type, colorless to light yellow transparent liquid, miscible with epoxy resin, low viscosity at room temperature, high boiling point, non-volatile, non-toxic, non-irritant, safe for operation and use. It is a good diluent for epoxy resin.YLD-2005 is cured with epoxy resin, and there is a long chain of flexible fat in the molecular structure, which can be rotated freely and is elastic.YLD-2005 can be added to epoxy resin formula to greatly improve its impact strength and resistance to cold and hot impact, and improve the brittle cracking defects of the epoxy cured material.

 

 

 

 

Item

YLD-2005A

YLD-2005B

Appearance

Transparent liquid

Transparent liquid

Color, APHA

Max. 40

Max. 60

Viscosity, mpa.s 25°C

30-50

40-70

EEW, g/eq

285-335

335-435

Hydrolyzable Chloride,%

Max. 0.3

Max. 0.3

Inorganic Chlorine, mg/kg

Max. 20

Max. 20

Water,%

Max.0.1

Max.0.1

 

  • YLD-2005 can be used to formulate all kinds of epoxy resin castables, solvent-free coatings, impregnating adhesives, drop-dipping adhesives and adhesives.

  • YLD-2005 is widely used in the manufacture of high-voltage switching parts of large and medium-sized dry-type transformer transformers, micro-motors, capacitors and other electronic devices.

  • YLD-2005 is also the main component of automobile electrophoretic coating.

 

Store in well-ventilated area. Keep away from flames and direct sunlight. Close the cap tightly immediately after use.

All safety information is provided in the Material Safety Data Sheet.

 

At least 12 months from the date of manufacture in the original packing in ambient temperatures.

 

Drum package.

 

leave a message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.
Hot Products

Related Products

Diluent sample
Triethylene Glycol Divinyl Ether YLD-S0102

YLD-S0102, chemical name Triethylene Glycol Divinyl Ether, CAS No. 765-12-8.

Diluent sample
Diethylene Glycol Divinyl Ether YLD-S0101

YLD-S0101, chemical name Diethylene Glycol Divinyl Ether, CAS No. 764-99-8.

Diluent sample
High-Flexibility Cardanol Diglycidyl Ether YLD-9016

YLD-9016, chemical name Cardanol Diglycidyl Ether, CAS No. 68390-54-5.

Diluent sample
Low-Viscosity Enhanced Cardanol Diglycidyl Ether YLD-9014A

YLD-9014A, chemical name Cardanol Diglycidyl Ether, CAS No. 68390-54-5.

Diluent sample
General-Purpose Standard Cardanol Diglycidyl Ether YLD-9014

YLD-9014, chemical name Cardanol Diglycidyl Ether, CAS No. 68390-54-5.

Diluent sample
Diethylene glycol diglycidyl ether YLD-2003

YLD-2003, chemical name Diethylene glycol diglycidyl ether, CAS No. 39443-66-8.

Diluent sample
Polypropylenglycol diglycidyl ether YLD-2005

YLD-2005, chemical name Polypropylenglycol diglycidyl ether, CAS No. 26142-30-3.

Diluent sample
2-Methylphenyl Glycidyl ether YLD-6002

YLD-6002, chemical name 2-Methylphenyl Glycidyl ether, CAS No. 2210-79-9.

Diluent sample
4-tert-Butylphenyl glycidyl ether YLD-6004

YLD-6004, chemical name 4-tert-Butylphenyl glycidyl ether, CAS No. 3101-60-8.

Diluent sample
(C8-10)alkylglycidyl ether YLD-7004

YLD-7004, chemical name (C8-10)alkylglycidyl ether, CAS No. 68609-96-1.

Diluent sample
Allyl glycidyl ether YLD-9005

YLD-9005, chemical name Allyl glycidyl ether, CAS No.106-92-3. 

Diluent sample
Tetrahydrophthalic acid diglycidylester YLD-9012

YLD-9012, chemical name Tetrahydrophthalic acid diglycidylester, CAS No. 21544-03-6.

Diluent sample
N N-DIGLYCIDYLANILINE YLD-9013

YLD-9013, chemical name N,N-Diglycidylphenylamine, CAS No. 2095-06-9.

Diluent sample
Cardanol glycidyl ethers YLD-9006

YLD-9006, chemical name Cardanol glycidyl ethers, CAS No. 171263-25-5.

Diluent sample
Butyl glycidyl ether(BGE) YLD-9004

YLD-9004, chemical name Butyl glycidyl ether(BGE), CAS No. 2426-08-6. 

Diluent sample
Neopentyl glycol diglycidyl ether YLD-6009

YLD-6009, chemical name Neopentyl glycol diglycidyl ether, CAS No. 17557-23-2.

Diluent sample
1,4-Butanediol diglycidyl ether YLD-6018L

YLD-6018L, chemical name 1,4-Butanediol diglycidyl ether, CAS No. 2425-79-8.

Diluent sample
1,6-Hexanediol diglycidyl ether YLD-6008

YLD-6008, chemical name 1,6-Hexanediol diglycidyl ether, CAS No. 16096-31-4. 

Diluent sample
Benzyl glycidyl ether YLD-6021

YLD-6021, chemical name Benzyl glycidyl ether, CAS No. 89616-40-0.

Diluent sample
Glycidyl phenyl ether YLD-6001

YLD-6001, chemical name Glycidyl phenyl ether, CAS No. 122-60-1. 

Diluent sample
Castor oil glycidyl ether YLD-9003

YLD-9003, chemical name Castor oil glycidyl ether, CAS No. 74398-71-3. 

Diluent sample
1,2,3-Propanetriol glycidyl ether YLD-6011

YLD-6011, chemical name 1,2,3-Propanetriol glycidyl ether, CAS No. 13236-02-7.

Diluent sample
Pentaerythritol glycidyl ether YLD-6013

YLD-6013, chemical name Pentaerythritol glycidyl ether, CAS No. 3126-63-4. 

Diluent sample
Resorcinol diglycidyl ether YLD-6010

YLD-6010, chemical name Resorcinol diglycidyl ether, CAS No. 101-90-6. 

Diluent sample
Trimethylolpropane triglycidyl ether YLD-6012

YLD-6012, chemical name Trimethylolpropane triglycidyl ether, CAS No. 30499-70-8. 

Diluent sample
Neodecanoic acid glycidyl ester YLD-8001

YLD-8001, chemical name Neodecanoic acid glycidyl ester, CAS No. 26761-45-5. 

Diluent sample
Alkyl (C12-C14) glycidyl ether YLD-7003

YLD-7003, chemical name Alkyl (C12-C14) glycidyl ether, CAS No. 68609-97-2. 

Diluent sample
Hexahydro-phthalic acid diglycidylester YLD-8003

YLD-8003, chemical name Hexahydro-phthalic acid diglycidylester, CAS No. 5493-45-8. 

leave a message

leave a message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.
submit

home

products

WhatsApp

Contact Us