Language :
![]()
Bisphenol A epoxy resin, chemical name bisphenol A diglycidyl ether, is made by the reaction of bisphenol A and epichlorohydrin under alkaline conditions. Bisphenol A epoxy resin is the largest production of epoxy resins, but also one of the most widely used varieties. Because of its good physical and mechanical properties, chemical resistance and electrical insulation properties, epoxy resin is widely used in coatings, adhesives, glass fibre reinforced plastic, laminates, electronic casting, potting, encapsulation and other fields.
![]()
Bisphenol A liquid epoxy resin comparing with most resins, its cured product has higher adhesion strength, lower shrinkage, especially outstanding performance in mechanical strength, electrical insulation, and chemical resistance.
![]()
| Grade No. | EEW (g/eq) |
Viscosity (mPa.s) |
N.V. (%) |
| YLE-128A90 | 184-194 | ≤1000 | 90±1 |
| YLE-128X90 | 184-194 | 500-1000 | 90±1 |
| YLE-134X80 | 230-270 | 500-1500 | 80±1 |
| YLE-136X80 | 290-335 | 3500-7000 | 80±1 |
| YLE-901X75 | 450-550 | 7000-15000 | 75±1 |
| YLE-901A80 | 450-550 | 1500-4000 | 80±1 |
| YLE-902X75 | 600-700 | 20000-50000 | 75±1 |
![]()
Adhesive
Insulation
Composites (Glass fiber, carbon fiber winding material)
Coating
Electrical and electronic industry (Potting, casting, impregnation)
Civil wood bedding
![]()
Store in well-ventilated area. Keep away from flames and direct sunlight. Close the cap tightly immediately after use.
All safety information is provided in the Material Safety Data Sheet.
![]()
At least 12 months from the date of manufacture in the original packing in ambient temperatures.
![]()
Drum package.