1,3-cyclohexanedimethylamine CAS No.579-20-6,short for 1,3-BAC,is used as a raw material for epoxy resin curing agents in a wide range of applications around the world.

1,3-BAC, as an alicyclic amine, has excellent hardness, weathering, and chemical resistance, a refined appearance, and a faster cure rate.

 

Typical Physical and Chemical Data

  • Appearance: Colourless transparent liquid
  • Colour (G):1.0 Max
  • Viscosity (mPa.s/20℃): 9.1
  • Active hydrogen equivalent(g/eq): 35.6

 

Advantages of 1,3-BAC as an epoxy resin curing agent

  • Excellent UV resistance and transparency
  • Fast curing speed
  • Excellent curing at high temperatures & high humidity
  • Low active hydrogen equivalents, low additions
  • Low solidification point
  • Good curing even at low temperatures.

 

Application of 1,3-BAC

     In jewellery adhesive

  • 1,3-BAC's excellent resistance to yellowing provides a long-lasting guarantee for the glossy appearance of the jewellery adhesive.
  • 1,3-BAC provides hardness guarantee for jewellery.
  • 1,3-BAC lower addition faster curing speed to improve the overall cost-effective advantage.

     In seam sealer

  • Improve the curing speed, 1,3-BAC can fully guarantee the curing time.
  • 1,3-BAC low colour, high transparency to fully guarantee the appearance of the product colour.
  • 1,3-BAC provides the required hardness and strength to the product.

    In composite materials

  • 1,3-BAC low active hydrogen equivalent, low additive quantity can bring higher cost-effective advantage for products.
  • 1,3-BAC high hardness, to provide assurance for the strength of the product.
  • 1,3-BAC good chemical resistance, to ensure that the product's lasting use.

    In laminating adhesive

  • 1,3-BAC's excellent resistance to yellowing provides assurance of long-lasting colour stability of the cured product.
  • 1,3-BAC's excellent colour transparency ensures the transparent and clear quality of the product.
  • The low viscosity of 1,3-BAC ensures good workability.

 

1,3-BAC (1,3-cyclohexanedimethylamine) is now widely used as epoxy resin curing agent in coatings, adhesives, composites, etc. 1,3-BAC is one of the amines with less additive quantity at present, and its excellent product appearance and performance make it have an outstanding cost-effective advantage.

 

Nanjing Yolatech provides all kinds of high purity and low chlorine epoxy resins, including Bisphenol A epoxy resin, Bisphenol F epoxy resin, Phenolic epoxy resin, Brominated epoxy resin, DOPO modified phenolic epoxy resin, MDI modified epoxy resin, DCPD epoxy resin, Multifunctional epoxy resin, Crystalline epoxy resin, HBPA epoxy resin and so on. And we also could provide all kinds of epoxy resin curing agents or hardeners and diluents.

 

We will be at your service 24 hours a day. Pls contact us freely.

 

leave a message

leave a message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.
submit

home

products

WhatsApp

Contact Us