1. Product Information
|
Item |
Information |
|
Chemical Name |
1,3-Benzenedimethanamine Reaction Products with Epichlorohydrin |
|
Product Code |
1,3-BDX |
|
CAS No. |
135470-04-1 |
|
Category |
Modified amine epoxy curing agent |
|
Main Applications |
Epoxy coatings, floor coatings, industrial protective coatings, adhesives |
2. Product Description
1,3-BDX is a modified amine epoxy curing agent derived from MXDA. It is designed for epoxy curing systems that require good color stability, moderate viscosity, fast curing performance, wet surface adhesion and excellent chemical resistance.
In epoxy resin systems, 1,3-BDX can be used directly as a curing agent or combined with other amine curing agents to improve processability, adjust curing speed and enhance corrosion resistance and water resistance of cured products. It is suitable for floor coatings, industrial protective coatings and adhesive systems requiring adhesion and durability.
3. Structure Features and Key Advantages
3.1 Structure and Reactivity
1,3-BDX is based on an MXDA-derived modified amine system. It retains amine reactivity toward epoxy resin while improving compatibility and application stability. Compared with conventional low-molecular amine curing agents, it offers a balanced profile of processability, wet surface adhesion, later-stage curing speed and resistance properties.
3.2 Key Advantages
· Good color stability for appearance-sensitive coatings and adhesives.
· Moderate viscosity for easier mixing with epoxy resin and formulation adjustment.
· Fast curing performance to improve application efficiency and shorten curing time.
· Good wet surface adhesion for demanding application conditions.
· Excellent corrosion and water resistance for long-term durability.
· Flexible formulation use: suitable for direct use or blending with other curing agents as an accelerator or performance modifier.
4. Technical Data
|
Item |
Typical Value |
|
Appearance |
Clear liquid |
|
Color, Gardner |
≤5 |
|
Viscosity, cps @25°C |
7000-14000 |
|
Total Amine, mg KOH/g |
650-680 |
|
MXDA Content, % |
24-30 |
Note: The above values are typical data for product identification and formulation reference only. They should not be considered as a performance guarantee. End users should conduct their own tests based on specific resin systems, formulations and application conditions.
5. Applications

5.1 Epoxy Floor Coatings
1,3-BDX can be used in epoxy floor coating systems to support processability, curing speed, wear resistance, water resistance and chemical resistance.
5.2 Industrial Protective Coatings
It is suitable for industrial equipment, concrete substrates and metal protection, helping improve adhesion, corrosion resistance and long-term durability.
5.3 Adhesive Systems
It can be used in industrial adhesive or structural adhesive systems requiring adhesion, water resistance and chemical resistance.
5.4 Blended Curing Systems
1,3-BDX can be blended with other amine curing agents as a curing accelerator or performance modifier to balance pot life, curing speed and final properties.
6. Packaging, Storage and Safety
|
Item |
Information |
|
Packaging |
Drums; IBC tanks |
|
Storage Temperature |
5-30°C |
|
Storage Conditions |
Keep sealed in a cool and dry place. Avoid direct sunlight. |
|
Avoid Contact |
Strong oxidants and acids |
|
Storage Life |
12 months from the date of manufacture in the original packing under ambient temperatures |
|
Safety |
Refer to MSDS for detailed handling, transportation and safety information |
7. Sales Keywords
1,3-BDX supplier; epoxy curing agent supplier; MXDA modified curing agent; floor coating hardener; industrial coating curing agent; epoxy adhesive hardener