1,3-Cyclohexanedimethylamine (1,3BAC) epoxy resin curing agent

1,3-Cyclohexanedimethylamine (1,3BAC) epoxy resin curing agent
June 20, 2024

Product information

1.3-BAC is a diamine substance, it is colourless transparent and low viscosity liquid at room temperature, it has obvious ammonia smell, corrosive and combustible when it meets open fire. It belongs to cyclic aliphatic amine, when used as epoxy curing agent, it has both the high activity of aliphatic amine and the excellent mechanical properties, temperature resistance and yellowing resistance of alicyclic amine, it is often used in the preparation of high-quality epoxy adhesive products.

 

Application

Mainly used as epoxy curing agent or preparation of modified epoxy curing agent, not only low viscosity, good operability, and excellent room temperature curing performance, its products in the mechanical properties, temperature resistance, water resistance, chemical resistance and other aspects of the excellent preparation of high-quality epoxy adhesives, flooring paints, etc., are widely used in high-end flooring, jewelry adhesive, crystal adhesive, stone adhesive industry; at the same time, due to its excellent mechanical properties, good operability, also used in composite materials. At the same time, due to its excellent mechanical properties and good operability, it is also used in composite material industry (automobile, wind blade, etc.).

 

Ratio

Epoxy resin 128 (epoxy equivalent 190):100

Amount of curing agent: 17~20

 

Nanjing Yolatech provides all kinds of high purity and low chlorine epoxy resins, including Bisphenol A epoxy resin, Bisphenol F epoxy resin, Phenolic epoxy resin, Brominated epoxy resin, DOPO modified phenolic epoxy resin, MDI modified epoxy resin, DCPD epoxy resin, Multifunctional epoxy resin, Crystalline epoxy resin, HBPA epoxy resin and so on. And we also could provide all kinds of curing agents or hardeners and diluents.

 

We will be at your service 24 hours a day. Pls contact us freely.

 

leave a message

leave a message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.
submit

home

products

WhatsApp

Contact Us