Home blog

Application of Polyetheramine in Epoxy Terrazzo Flooring

Application of Polyetheramine in Epoxy Terrazzo Flooring
April 11, 2024

Epoxy terrazzo flooring is produced using epoxy resin and curing agents as binders, supplemented with various decorative aggregates, and manufactured through special processes. Epoxy terrazzo flooring can be widely applied in large-scale shopping malls, high-end commercial buildings, luxury clubs, exhibition halls, hotel lobbies, as well as residential and villa floor decorations. Epoxy terrazzo flooring features moisture resistance, slip resistance, waterproofing, dust prevention, and durability.

Polyetheramine products used as curing agents in epoxy terrazzo flooring

Polyetheramine D-230

Polyetheramine D-230 is a bifunctional amine with an average molecular weight of about 230.

Features:

  • Low viscosity, low color, low volatility
  • Fully miscible with various solvents, including water
  • The cured product is tough, clear, and has excellent impact resistance, suitable for coatings, casting, adhesives, etc.
  • The coating surface does not exhibit common whitening phenomena associated with the use of other amine curing agents

Typical Data:

  • Appearance: Colorless and transparent
  • Average active hydrogen equivalent (g/eq): ~60
  • Color (Pt-Co): ~25
  • Viscosity (cst, 25℃): ~9.5                                                                                                                                                       

 

Nanjing Yolatech provides all kinds of high purity and low chlorine epoxy resins, including Bisphenol A epoxy resin, Bisphenol F epoxy resin, Phenolic epoxy resin, Brominated epoxy resin, DOPO modified phenolic epoxy resin, MDI modified epoxy resin, DCPD epoxy resin, Multifunctional epoxy resin, Crystalline epoxy resin, HBPA epoxy resin and so on. And we also could provide all kinds of curing agents or hardeners and diluents.

We will be at your service 24 hours a day. Pls contact us freely.

 

 

leave a message

leave a message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.
submit

home

products

WhatsApp

Contact Us