Application of Epoxy Resin in Concrete Crack Reinforcement Adhesive
                                        
										                                                    Apr 18, 2024
                                                									
                                        
                                            Epoxy resin adhesive is a widely used chemical grouting materials, epoxy resin adhesive with high strength, good adhesive force, low curing shrinkage, in line with a variety of process needs, can meet the needs of concrete crack repair. Epoxy resin and polyamide as the main film-forming substances, compound diluent, accelerator, etc. made of glue, according to the gap, supplemented by atmospheric pressure or high pressure grouting method will be injected into the cracks, so as to achieve adhesion, reinforcing, seepage and other repair effects.
 
Here we introduce two commonly used epoxy resin products, used in concrete reinforcement, with good adhesive strength, levelling performance and excellent mechanical properties.
 
YL-128
Epoxy equivalent (g/eq): 184 ~ 190
 
Viscosity (cps/25℃): 12000 ~ 15000
 
Product Description: Standard bisphenol A epoxy resin for general use.
 
YL-127
Epoxy equivalent (g/eq): 176 ~ 184
 
Viscosity (cps/25℃): 8000 ~ 11000
 
Product Description: Low viscosity standard bisphenol A epoxy resin.
 
Nanjing Yolatech provides all kinds of high purity and low chlorine epoxy resins, including Bisphenol A epoxy resin, Bisphenol F epoxy resin, Phenolic epoxy resin, Brominated epoxy resin, DOPO modified phenolic epoxy resin, MDI modified epoxy resin, DCPD epoxy resin, Multifunctional epoxy resin, Crystalline epoxy resin, HBPA epoxy resin and so on. And we also could provide all kinds of curing agents or hardeners and diluents.
We will be at your service 24 hours a day. Pls contact us freely.
                                        
                                                                                    