  • Benzyl Glycidyl Ether YLD-6021: Low-Odor Epoxy Diluent
    Benzyl Glycidyl Ether YLD-6021: Low-Odor Epoxy Diluent
    Nov 16, 2026
    Benzyl glycidyl ether YLD-6021 is a monofunctional aromatic diluent at 208-228 g/eq and 2-8 mPa·s, picked for potting when colour and chloride allow. At 20 phr it lifts blend EEW so amine demand falls, not rises; the same load brings 750 ppm hydrolyzable chloride, and that number settles the choice. Figure 1. YLD-6021 is a water-clear liquid; the published colour ceiling is APHA 50. 1. Introduction Viscosity limits most room-temperature epoxy work. A liquid bisphenol A resin such as YLE-128 runs at 11,000-15,000 mPa·s, too thick for potting fine windings or a brush coat without solvent. A reactive diluent lowers that figure and stays in the film. Several diluents in this catalogue bring that figure down, and choosing between them on viscosity alone is a mistake: functionality, colour ceiling and chloride load move with the choice. This report sets benzyl glycidyl ether YLD-6021 (CAS 89616-40-0) against three of them and states the arithmetic behind each decision. 2. Materials and Methods: Benzyl Glycidyl Ether YLD-6021 Specification 2.1 Product Identification The CAS number sits in the product page intro line, not the specification table. Table 1. Identity of benzyl glycidyl ether YLD-6021. Item Information Chemical name Benzyl glycidyl ether CAS No. 89616-40-0 Molecular formula C10H12O2 (calculated) Molecular weight 164.20 g/mol (calculated) Theoretical EEW 164.2 g/eq, one oxirane per molecule (calculated) Appearance Transparent liquid Package Drum 2.2 Specification Data and Test Methods Seven parameters are published, with no cure data and no thermal properties. Table 2. Published specification of YLD-6021 with the method applied to each parameter. Parameter Published value Method Colour, APHA Max. 50 APHA scale Viscosity at 25 °C, mPa·s 2-8 ASTM D445 EEW, g/eq 208-228 ASTM D1652, ISO 3001 Hydrolyzable chloride, % Max. 0.2 Titration Inorganic chlorine, ppm Max. 50 Titration Water, % Max. 0.1 ASTM E203 Epoxy equivalent weight is determined by titration according to ASTM D1652 or ISO 3001, water content according to ASTM E203. Viscosity is quoted at 25 °C; the page names no method, and ASTM D445 is the standard used across this catalogue. With no standard deviation or replicate count published, these figures are limits, not typicals. The published EEW of 208-228 g/eq sits well above the 164.2 g/eq calculated for the pure monomer, and that gap decides the arithmetic. A grade at 218 g/eq carries about three quarters of the epoxy content of the pure monomer; the rest is non-reactive. Substituting 164 overstates epoxy equivalents by a third, and the hardener weight follows. 3. Results and Discussion: Structure and Reactivity of Benzyl Glycidyl Ether 3.1 Why the Viscosity Falls So Far Benzyl glycidyl ether carries one oxirane ring on a short ether chain capped by a benzene ring, and no hydroxyl. That absence is why viscosity lands at 2-8 mPa·s. Bisphenol A resin is thick because its backbone hydroxyls hydrogen-bond; a benzyl ether has nothing to bond with. At 15 phr it takes a 13,000 mPa·s resin to about 4,660 mPa·s, the working range for casting small housings (Table 5). Reactivity is where the monofunctionality costs. Each molecule reacts once and stops, capping a chain end rather than extending the network, so crosslink density falls with the monofunctional fraction. The aromatic ring recovers part of that, and the page claims a high heat deflection temperature without publishing an HDT value to size it. 3.2 Selection Matrix Against Three Diluents Table 3 lines YLD-6021 up against three grades; all colour values are APHA, not Gardner. Table 3. Selection matrix: benzyl glycidyl ether YLD-6021 against three diluents, values as published on each product page. Property YLD-6021 YLD-6001 YLD-9004A Chemical type Benzyl glycidyl ether Glycidyl phenyl ether Butyl glycidyl ether Functionality 1 1 1 EEW, g/eq 208-228 Not published 147-157 Viscosity at 25 °C, mPa·s 2-8 2-8 Max. 2 Colour, APHA Max. 50 Max. 50 Max. 20 Hydrolyzable chloride Max. 0.2 % Not published Max. 0.1 % Effect on blend EEW Raises Raises Lowers The last two rows drive the pick. Difunctional 1,6-hexanediol diglycidyl ether YLD-6008 at 142-155 g/eq pulls blend EEW down and hardener demand up; YLD-6021 at 218 g/eq does the opposite. At 20 phr the two recipes need 12.9 phr against 11.5 phr, a gap no batch sheet shows. Odour and colour settle the rest. Butyl glycidyl ether YLD-9004A reaches max. 2 mPa·s at APHA 20, both better than YLD-6021, and pays with a sharper smell on an open line. Table 4 orders them by cost of getting them wrong. Table 4. Diluent decision sequence for a room-temperature bisphenol A system: condition, action, governing limit. Application condition Action Governing limit Ionic limit under 500 ppm Stop; settle the COA first 2,000 ppm hydrolyzable Cl Light or white topcoat Move to YLD-9004A APHA 50 vs APHA 20 Crosslink density first Use difunctional YLD-6008 Monofunctional capping Open pot, operators close Keep YLD-6021, skip the butyl Odour claim: neat liquid Target 3,000-5,000 mPa·s Set 15-20 phr Log mixing rule, coupon check Structural part over 20 phr Reduce loading or accept lower HDT A quarter of binder capped 4. Formulation and Dosage Calculation Once the grade is fixed, hardener demand follows the epoxy equivalents in the blend, not the resin mass alone. EEW(blend) = (100 + L) ÷ (100 ÷ EEW(resin) + L ÷ EEW(diluent)), with L as diluent loading in phr phr(amine) = 100 × AHEW ÷ EEW(blend) Table 5 applies both to liquid bisphenol A epoxy resin YLE-128 (EEW 184-190 g/eq, 11,000-15,000 mPa·s) with YLD-6021 at 0-30 phr. Viscosity comes from the logarithmic mixing rule, an approximation to check on a coupon before scaling. Table 5. Blend properties of YLD-6021 in YLE-128; viscosity estimated, hardener calculated at AHEW 20.6 g/eq. YLD-6021, phr Blend EEW, g/eq Viscosity, mPa·s DETA, phr blend DETA, phr resin 0 187.0 13,000 11.0 11.0 5 188.3 8,940 10.9 11.5 10 189.4 6,360 10.9 12.0 15 190.5 4,660 10.8 12.4 20 191.5 3,510 10.8 12.9 30 193.3 2,120 10.7 13.9 A 120 kg batch of 100 kg YLE-128 plus 20 kg YLD-6021 lands at 191.5 g/eq and takes 12.9 kg of diethylenetriamine at AHEW 20.6 g/eq, or 10.75 phr on blend mass. Both describe one recipe; quoting one without its basis is the usual dosing error at scale. Chloride scales with loading. At 20 phr the diluent brings about 40 g of hydrolyzable chloride into that batch against 50 g from the resin, near 750 ppm; at 30 phr, 846 ppm. With an ionic limit under 500 ppm neither loading passes, and the COA value has to be settled first. Twenty phr is a sensible ceiling for structural work. At 30 phr viscosity falls to 2,120 mPa·s, but a quarter of the binder is monofunctional and heat distortion shows it. 5. Processing Notes and Operating Window YLD-6021 disperses without high shear, which changes the sequence, not the equipment. Add the diluent to resin at 40-50 °C and stir slowly; high shear pulls in air that the liquid then holds. Weigh by mass. Density is not published, so a volume guess can be 5 % out and the EEW arithmetic with it. Keep the drum closed; a drum left open in a humid room picks up water, and 0.1 % is not generous. Do not hold a batch past gel time; a thin blend gives no visual warning. Figure 2. Diluent is metered into the resin by mass; low-shear mixing is enough at 2-8 mPa·s. A 20 phr blend holds less resin per unit volume, so a thick casting runs cooler while a thin film skins sooner. Re-check the cure schedule when loading changes. 6. Applications Three uses appear on the page, each loading following from Table 4. Table 6. Applications of YLD-6021, with the loading it supports and the governing limit. Application Role in the process Loading, phr Governing limit Electronic potting Cavity fill and wetting of windings 10-20 Hydrolyzable chloride budget Coating Solvent-free let-down for brush or roller 15-25 Colour ceiling at APHA 50 Construction adhesive Penetration into rough substrate 10-15 Chain termination at high load Figure 3. Potting a wound assembly: 10-20 phr of YLD-6021 brings a bisphenol A system into the 3,500-6,400 mPa·s range. Potting is the demanding case. A 20 phr blend at 3,510 mPa·s wets a winding in one pass, but it carries 750 ppm hydrolyzable chloride, and that number, not viscosity, decides insulation tests on high-impedance circuits. 7. Limitations and Material Verification 7.1 Where the Grade Does Not Fit Four limits rule uses out, each a selection filter. Monofunctional by design: a viscosity tool, not a crosslinker, and it will not carry a high-Tg formulation alone. Hydrolyzable chloride at max. 0.2 %, or 2,000 ppm, is the highest in its family; YLD-9004A allows 0.1 %. No thermal, mechanical or electrical data are published: no Tg, no HDT, no dielectric strength. EEW 208-228 g/eq against a theoretical 164.2 means composition is not fixed; check viscosity and EEW each lot. The 4-tert-butylphenyl glycidyl ether YLD-6004 page repeats the 2-methylphenyl description word for word, so verify that grade from its table alone. 7.2 Incoming Inspection, Packaging, Storage and Safety Incoming check covers viscosity at 25 °C, colour, water and EEW on the COA sample. Viscosity and EEW catch most off-spec lots; a wet batch shifts in viscosity before the water figure moves. Drums keep 12 months in original packing at ambient temperature, away from flame and sunlight. Safety data sits in the Material Safety Data Sheet; treat the liquid as a skin sensitiser until the MSDS says otherwise. No RoHS or REACH status is claimed here; that comes from the supplier's declaration. 8. Frequently Asked Questions When should YLD-6021 be chosen over another reactive diluent? Choose it when the ionic limit sits above 500 ppm, the topcoat is not colour-critical and Tg can give up a little: it is the only grade here that cuts viscosity while lowering amine demand. Move to YLD-9004A for APHA 20, or YLD-6008 when crosslink density beats flow. How much YLD-6021 should be added to an epoxy resin? Ten to twenty phr covers most work. At 20 phr a 13,000 mPa·s resin drops to 3,500 mPa·s; 30 phr reaches 2,120 mPa·s but makes a quarter of the binder monofunctional. Is YLD-6021 the same as butyl glycidyl ether? No. YLD-6021 is benzyl glycidyl ether, CAS 89616-40-0, at EEW 208-228 g/eq; YLD-9004A is butyl glycidyl ether, CAS 2426-08-6, at 147-157 g/eq. Both are monofunctional, but blend EEW moves opposite ways. Does YLD-6021 lower the glass transition temperature? Yes. Capping chain ends drops crosslink density and Tg together. How far depends on the hardener, since the page lists no Tg or HDT; the aromatic ring offsets part of it, and a coupon settles the rest. What chloride load does YLD-6021 bring into a potting compound? The specification allows max. 0.2 % hydrolyzable chloride, or 2,000 ppm. At 20 phr in a resin carrying 500 ppm the blend lands near 750 ppm; at 30 phr, 846 ppm. Can YLD-6021 replace solvent in a solvent-free coating? It can, and it stays in the film, so there is no flash-off step and no diluent VOC. Two constraints apply: hardness drops at high loading, and APHA 50 bars light topcoats that the butyl grade would pass. 9. Conclusions Benzyl glycidyl ether YLD-6021 cuts viscosity to 2-8 mPa·s while moving blend EEW up, so amine demand falls as loading rises — the reverse of difunctional grades. At 20 phr in YLE-128 the blend reaches 191.5 g/eq and 3,500 mPa·s, needing 12.9 kg of diethylenetriamine per 100 kg of resin. Selection then turns on two limits, not viscosity. Chloride at 2,000 ppm puts the blend at 750 ppm at 20 phr, ruling out high-impedance potting unless the COA comes lower; chain termination rules out structural parts above 20 phr. 10. References 1. Yolatech product page: https://www.yolatech.com/benzyl-glycidyl-ether-yld-6021 (accessed 2026-11-16). 2. Yolatech Technical Data Sheet (TDS) for YLD-6021, benzyl glycidyl ether, CAS 89616-40-0, on request. 3. Yolatech Certificate of Analysis (COA) for YLD-6021, batch values, on request. 4. ASTM D1652, epoxy content of epoxy resins (EEW). 5. ISO 3001, determination of epoxy equivalent. 6. ASTM D445, kinematic viscosity. 7. ASTM E203, water content by Karl Fischer titration.
    Read More
  • Bio-Based Epoxy Reactive Diluent: YLD-9016 Dosage Guide
    Bio-Based Epoxy Reactive Diluent: YLD-9016 Dosage Guide
    Oct 14, 2026
    Bio-based epoxy reactive diluent YLD-9016 is a difunctional cardanol diglycidyl ether specified at EEW 250-330 g/eq and 60-150 mPa·s at 25 °C. CAS 68390-54-5, non-volatile content 99.7% minimum, derived from cashew nut shell liquid. At 15 phr the diluent cuts a 13000 mPa·s resin to about 6300 mPa·s. Figure 1. Cardanol diglycidyl ether YLD-9016 is supplied as a light yellowish brown liquid with a Gardner color of 12 maximum and ships in 200 kg drums. 1. Introduction A high-solids epoxy formulation needs its viscosity cut by something that stays in the film. Solvent leaves as VOC; a reactive diluent cures into the network instead. That is the argument for glycidyl ethers. The cardanol line already covers three answers: cardanol glycidyl ethers YLD-9006 monofunctional at 30-50 mPa·s, and standard cardanol diglycidyl ether YLD-9014 with its variant YLD-9014A difunctional but at 1000-3000 mPa·s. Resin-class flow, not diluent-class flow. YLD-9016 publishes 60-150 mPa·s with two epoxy groups per molecule. It is the only grade in the family that pairs diluent-class viscosity with difunctional reactivity, on a cashew-derived backbone. Viscosity is only half the argument. Specification values below come from the public Yolatech product pages, derived constants are marked calculated, and dosage figures are worked examples. 2. Materials and Methods: Identification of Bio-Based Epoxy Reactive Diluent YLD-9016 Table 1 collects the identity and specification data published for YLD-9016. 2.1 Product Identification and Specification Table 1. Identity and published specification of bio-based epoxy reactive diluent YLD-9016. Item Information Product name Cardanol Diglycidyl Ether YLD-9016 Chemical family Cashew oil modified difunctional glycidyl ether CAS No. 68390-54-5 Appearance Light yellowish brown liquid Color, G Max. 12 EEW, g/eq 250-330 Viscosity (25 °C), mPa·s 60-150 Non-volatile, % Min. 99.7 Epoxy functionality 2 (bifunctional, as published) Raw material base Cashew nut shell liquid, plant-derived Packaging 200 kg drum Shelf life 12 months in original packing 2.2 Test Methods and Data Sources Table 1 reproduces the published figures without alteration. The report adds no laboratory data of its own. Epoxy equivalent weight is determined by titration under ASTM D1652 or ISO 3001, and the figure on the current TDS governs. Color is determined by ASTM D1544, and viscosity is measured at 25 °C under the method stated in the current TDS. Incoming checks on a glycidyl ether lot are typically run in duplicate, or as n = 3 determinations from separate positions in the drum. 3. Results and Discussion: Viscosity, Functionality and Dilution Behaviour Two published numbers separate YLD-9016 from the cardanol line: 60-150 mPa·s at 25 °C and 99.7% minimum non-volatile. 3.1 Structure and Reactivity of the Cardanol Backbone Cardanol is a meta-substituted phenol carrying a C15 unsaturated alkyl chain, obtained from cashew nut shell liquid. Capping that core with two glycidyl groups gives a rigid aromatic ring, a long hydrophobic tail and two reactive epoxide ends. Each part does one job. The epoxide ends consume amine and enter the network. The alkyl chain buys flexibility and water repellency. The aromatic ring lets a film harden at room and low temperatures. Nothing evaporates. A non-volatile content of 99.7% minimum means essentially the whole dose becomes part of the film. 3.2 Comparison with Alternative Systems Table 2 places YLD-9016 beside the petrochemical ethers it replaces and the sibling cardanol grades. Table 2. Property comparison of bio-based epoxy reactive diluent YLD-9016 with alternative reactive diluents (published values). Property YLD-9016 YLD-9014 AGE YLD-7003 BGE YLD-9004A HDDGE YLD-6008 Epoxy functionality 2 2 1 1 2 EEW, g/eq 250-330 290-350 294-313 147-157 142-155 Viscosity (25 °C), mPa·s 60-150 1000-3000 4-10 Max. 2 10-25 Raw material base Cashew, bio-based Cashew, bio-based Petrochemical Petrochemical Petrochemical Hardener demand vs 187 g/eq DGEBA Lowers Lowers Lowers Raises Raises   On raw thinning power the petrochemical ethers win: butyl glycidyl ether BGE YLD-9004 at 2 mPa·s maximum and 1,6-hexanediol diglycidyl ether YLD-6008 at 10-25 mPa·s, against 60-150 mPa·s. What they give back is hardener demand. At EEW 147-157 and 142-155 g/eq they pull a blend below the 184-190 g/eq of a standard bisphenol A resin, so every added part costs amine. YLD-9016 and alkyl (C12-C14) glycidyl ether YLD-7003 sit above 250 g/eq and push it down. Color limits are not comparable across the columns: the cardanol grades are limited in Gardner, the petrochemical ethers in APHA. Where a difunctional petrochemical ether is the incumbent, the product page names 1,4-butanediol diglycidyl ether YLD-6018L as a comparator, published at 98% minimum purity and no EEW window. 4. Formulation and Dosage Calculation Blend EEW and hardener demand follow two equations, with phr read as parts per hundred parts of resin by weight. Blend EEW = (100 + d) ÷ (100 ÷ EEW + d ÷ EEW9016), where d is the diluent loading in phr phr = 100 × AHEW ÷ EEW Table 3. Dilution and hardener dosage worksheet for 100 parts of bisphenol A epoxy resin YLE-128 at 187 g/eq and 13000 mPa·s, blended with YLD-9016 at its 290 g/eq and 105 mPa·s midpoints (calculated). YLD-9016 loading, phr Blend EEW, g/eq DETA phr at AHEW 20.6 MACM phr at AHEW 60 Viscosity estimate, mPa·s 0 187 11.0 32.1 13000 10 193 10.7 31.1 8400 15 196 10.5 30.6 6300 20 199 10.4 30.2 5800 Viscosity is estimated by a log-rule blend, which tracks glycidyl ether systems well enough for screening. A 15 phr loading takes an 11000-15000 mPa·s bisphenol A epoxy resin YLE-128 down to about 6300 mPa·s, a 51% cut. For a 1,000 g resin charge, weigh 150 g of YLD-9016 and 306 g of MACM curing agent at its published AHEW of 60 g/eq. Treat 30.6 phr as a starting point, because the 250-330 g/eq window is 80 g/eq wide. Dilution efficiency, not price, is the honest basis. No list price is published, so express the trade-off as viscosity reduction per phr and settle it against your own drum quotation. On that basis 15 phr of BGE reaches about 3500 mPa·s and wins on thinning, but YLD-9016 wins on volatile-free composition and hardener demand. If a formulation has to stay stiff, cap the loading near 20 phr and verify hardness development on the actual system. 5. Processing Notes and Operating Window Field practice with YLD-9016 reduces to five points. Add the diluent to the resin first and homogenize before the hardener enters; adding it after the amine invites stoichiometry errors. If a drum comes off a winter pallet, let it reach room temperature before reading viscosity, because the 60-150 mPa·s window is temperature-specific. Recalculate hardener phr from the lot COA each time a new drum arrives. Keep drums sealed between draws; glycidyl ethers absorb moisture slowly in humid storage, and water shows up later as blush. Run a gel-time check before locking pot life; difunctional diluents gel differently from the monofunctional ethers they replace. Figure 2. Diluent is poured into the resin and homogenized before the hardener is dosed, keeping the mix stoichiometry under control. 6. Applications The page lists high-solids and solvent-free coatings, adhesives and composites, plus surface alkylation of silica and titanium dioxide. Table 4. Application fit for bio-based epoxy reactive diluent YLD-9016 and the resin grades commonly blended with it. Application Why YLD-9016 fits Resin companion High-solids coatings Reactive dilution at 99.7% minimum non-volatile content YLE-128 Solvent-free 2K systems Co-cures into the network instead of leaving as emission YLE-170 Adhesives Flexibility, impact resistance and water resistance YLE-128 Composites and FRP Impregnation aid at diluent-class viscosity YLE-170 Filler surface treatment Alkylates silica and titanium dioxide surfaces None The coating logic runs through epoxy resin coatings: wherever a solvent-borne recipe converts to high solids, a reactive diluent with a negligible volatile fraction is the direct swap, but the hardener ratio still needs recalculating. Adhesive work is covered in epoxy resin adhesives, impregnation in epoxy resin composites. Figure 3. Solvent-free epoxy floor coating applied by roller, the application where reactive dilution replaces solvent entirely. 7. Limitations and Material Verification 7.1 Known Limitations and Unsuitable Cases Four specification gaps deserve confirmation before YLD-9016 is written into a purchase specification. Hydrolyzable chlorine, water content, density, flash point and molecular formula are not published; the grade gives only a non-volatile floor of 99.7%. Confirm them on the current TDS, MSDS and COA. The 250-330 g/eq EEW window is 80 g/eq wide, wider than the 184-190 g/eq of YLE-128. Batch drift inside it moves hardener demand by about 3% at a fixed loading. This grade is not the right choice for a stiff, heat-deflection-critical casting, and it is not a flame retardant: no halogen or phosphorus content is published. The food-grade statement appears on the YLD-9006 page, not here. Do not carry the claim across without written confirmation. 7.2 Incoming Inspection, Packaging, Storage and Safety Incoming inspection should confirm EEW by titration against the lot COA, plus color and non-volatile content. Reject a lot outside 250-330 g/eq. Packaging is a 200 kg drum with a stated shelf life of 12 months from manufacture in the original packing, stored cool and dry out of direct sunlight. Handling detail is carried by the Material Safety Data Sheet. Glycidyl ethers are skin sensitisers, so gloves and eye protection belong in the procedure. RoHS, REACH or UL 94 status has to be confirmed by the buyer against current certificates. A general product description implies no certification. 8. Frequently Asked Questions What is bio-based epoxy reactive diluent YLD-9016 made from? YLD-9016 is a cardanol diglycidyl ether derived from cashew nut shell liquid, with two epoxy groups per molecule. The page positions it as a non-toxic, renewable alternative to petrochemical ethers such as AGE and BGE. How is YLD-9016 different from YLD-9014 and YLD-9014A? The difference is viscosity. YLD-9016 runs at 60-150 mPa·s while YLD-9014 and YLD-9014A both sit at 1000-3000 mPa·s; all three share CAS 68390-54-5. How much YLD-9016 should be blended into a bisphenol A epoxy resin? Start between 10 and 20 phr. A log-rule estimate for 15 phr in an 11000-15000 mPa·s bisphenol A resin lands near 6300 mPa·s, and the right level depends on the stiffness the part can give up. Does YLD-9016 change the hardener dosage? Yes, downward. Its own EEW sits above the 184-190 g/eq of a standard bisphenol A resin, so each added part raises the blend EEW; at 15 phr the calculated MACM demand drops from 32.1 to 30.6 phr. Can YLD-9016 replace butyl glycidyl ether in a solvent-free coating? On thinning alone, no. BGE at 2 mPa·s maximum cuts deeper per phr and usually wins that comparison, so the swap makes sense when volatile content, odor or hardener demand carries more weight than the last third of the viscosity cut. Does YLD-9016 soften the cured coating? It adds flexibility by design, which is a trade rather than a defect. The alkyl chain lowers modulus and heat deflection while raising impact and water resistance, and the effect depends on the loading. 9. Conclusions Bio-based epoxy reactive diluent YLD-9016 is published at EEW 250-330 g/eq, 60-150 mPa·s at 25 °C, Gardner color 12 maximum and 99.7% minimum non-volatile content, in 200 kg drums with a 12-month shelf life. Its position is narrow but useful: diluent-class viscosity on a difunctional, cashew-derived backbone, with lower hardener demand than the petrochemical ethers it replaces. Dose by stoichiometry from the lot COA, cap the loading near 20 phr, and keep the deep-thinning monofunctional ethers for jobs that need them. 10. References 1. Product page, Cardanol Diglycidyl Ether YLD-9016, Yolatech: https://www.yolatech.com/cardanol-diglycidyl-ether-yld-9016 2. Product page, Cardanol Diglycidyl Ether YLD-9014, Yolatech: https://www.yolatech.com/cardanol-diglycidyl-ether-yld-9014 3. Product page, Butyl glycidyl ether BGE YLD-9004, Yolatech: https://www.yolatech.com/butyl-glycidyl-etherbge-yld-9004 4. Product page, 1,6-Hexanediol diglycidyl ether YLD-6008, Yolatech: https://www.yolatech.com/16-hexanediol-diglycidyl-ether-yld-6008 5. Product page, liquid bisphenol A epoxy resin YLE-127 / YLE-128, Yolatech: https://www.yolatech.com/bisphenol-a-epoxy-resin 6. Technical Data Sheet, Material Safety Data Sheet and Certificate of Analysis for Cardanol Diglycidyl Ether YLD-9016, Yolatech (available on request). 7. ASTM D1652 and ISO 3001, titration routes for epoxy content and epoxy equivalent weight. 8. ASTM D1544 for Gardner color, ASTM D445 for kinematic viscosity, ASTM E203 for water by Karl Fischer titration.
    Read More
  • Cardanol Diglycidyl Ether YLD-9014A: High-Reactivity Diluent
    Cardanol Diglycidyl Ether YLD-9014A: High-Reactivity Diluent
    Oct 04, 2026
    Cardanol diglycidyl ether YLD-9014A is a bio-based difunctional epoxy reactive diluent with EEW 200-270 g/eq and a viscosity of 1000-3000 mPa·s at 25°C. The cashew-oil grade cuts high-solid and solvent-free coatings and adhesives while holding film hardness and adding toughness and water resistance. Product Code: YLD-9014A CAS No.: 68390-54-5 Product Category: Diluent & Glycidyl Ether 1. Product Information YLD-9014A ships as a reddish brown liquid in 200 kg drums, with Gardner color max. 18 and water content max. 0.2%. The table below lists the published product data in one place. Item Information Product Code Cardanol Diglycidyl Ether YLD-9014A Chemical Name Cardanol diglycidyl ether, cashew oil modified difunctional glycidyl ether CAS No. 68390-54-5 Appearance Reddish brown liquid Color, G Max. 18 EEW, g/eq 200-270 Viscosity (25°C), mPa·s 1000-3000 Water, % Max. 0.2 Raw material base Cashew oil, plant-derived Packaging 200 kg drum Shelf life 12 months from date of manufacture, original sealed packing 2. Product Description: How Cardanol Diglycidyl Ether YLD-9014A Works Both ends of the cardanol molecule carry a glycidyl group, so YLD-9014A reacts into the cured network instead of evaporating out of it. That single detail is what separates a reactive diluent from a solvent. The backbone pairs a long hydrophobic alkyl chain with a rigid aromatic ring. The supplier describes the result as a balance among film flexibility, impact resistance, and hardness, which is a different promise from a plain flexibilizer that softens the coating to gain toughness. The specification number that separates YLD-9014A from the standard grade is EEW 200-270 g/eq against 290-350 g/eq. A lower epoxy equivalent weight packs more glycidyl groups into each kilogram of liquid, so a given dose of YLD-9014A contributes more crosslinking than the same dose of the standard cardanol diglycidyl ether. In practice that shows up as higher reactivity and a tighter cured network. When a formulation is short on cure speed or heat resistance, the lower-EEW grade buys some back without giving up the cardanol flexibility. It can be run blended into conventional epoxy resins, or as the standalone resin when flexibility is the priority. The raw material is a plant extract rather than a petrochemical feedstock, and the grade is presented as renewable and non-toxic. That helps in export markets where VOC reduction and bio-content carry weight in the specification. 3. YLD-9014A vs Alternative Reactive Diluents The realistic alternatives are the standard cardanol grade in the same family and the low-viscosity monofunctional ethers. Published specifications settle most of the choice before a trial batch is even mixed. Property YLD-9014A YLD-9014 YLD-9016 YLD-9006 BGE YLD-9004A Functionality Difunctional Difunctional Bifunctional Monofunctional Monofunctional EEW, g/eq 200-270 290-350 250-330 355-500 147-157 Viscosity (25°C), mPa·s 1000-3000 1000-3000 60-150 30-50 Max. 2 Raw material base Cashew oil, bio-based Cashew oil, bio-based Cashew oil, bio-based Cashew oil, bio-based Petrochemical Typical role Reactivity plus toughness in coatings and adhesives Standard general-purpose toughener-diluent High-flexibility, ultra-low viscosity Low-viscosity monofunctional diluent Fast, low-cost viscosity cut Every reactive diluent is a trade-off: flexibility and water resistance climb while Tg and hardness come down. If a film has to stay hard while you add impact resistance, the flexible-rigid balance of cardanol diglycidyl ether YLD-9014A fits better than a soft flexibilizer. When the job is a deep viscosity cut, the numbers are blunt. Cardanol diglycidyl ether YLD-9016 sits at 60-150 mPa·s and cardanol glycidyl ethers YLD-9006 at 30-50 mPa·s. YLD-9014A, at 1000-3000 mPa·s, is not the tool for that. Against petrochemical ethers, the honest comparison is odor and property retention. A butyl glycidyl ether BGE YLD-9004 thins faster and costs less per liter, but the cardanol grades are positioned as lower-odor options with less damage to cured thermal properties. For projects that also carry a halogen-free or low-odor requirement, that usually decides the argument. 4. Typical Technical Information of Cardanol Diglycidyl Ether YLD-9014A Cardanol diglycidyl ether YLD-9014A is specified by five published parameters: appearance, Gardner color, epoxy equivalent weight, viscosity, and water content. The values below are specification ranges, not batch certificates. Item Specification Appearance Reddish brown liquid Color, G Max. 18 EEW, g/eq 200-270 Viscosity (25°C), mPa·s 1000-3000 Water, % Max. 0.2 Confirm the current batch against the TDS, MSDS, and COA before releasing a formulation, and re-check EEW on incoming material if the hardener ratio is calculated tight. 5. Formulation and Selection Guidance Cardanol diglycidyl ether YLD-9014A carries epoxy groups of its own, so it consumes hardener like any other epoxide. Blend EEW = 1 / (w1/EEW1 + w2/EEW2), then hardener phr = 100 × AHEW / blend EEW. Worked example. Take 90 parts of a bisphenol F epoxy resin at EEW 170 plus 10 parts YLD-9014A at its EEW midpoint of 235 g/eq. Blend EEW = 1 / (90/170 + 10/235) = 175 g/eq. With a dicyandiamide-type hardener at AHEW 60, demand is 100 × 60 / 175 = 34.3 phr, against 35.3 phr for the neat resin. Treat 34.3 phr as a starting point, not a specification, because the exact figure depends on the accelerator package and cure schedule. Viscosity moves less than reactivity does, because YLD-9014A sits at 1000-3000 mPa·s itself. A log-rule estimate for 10 parts YLD-9014A taken at 2000 mPa·s in 90 parts of a 15,000 mPa·s resin lands near 12,300 mPa·s, roughly an 18% cut. If a line has to get under 1000 mPa·s, the ultra-low-viscosity grades are the correct pick instead. On dosage, most formulators start cardanol diglycidyl ether YLD-9014A at 5-15 phr against standard liquid epoxy resins. Above roughly 20 phr the network softens noticeably; check heat-deflection data on the actual system before committing to a level. We can supply grade-matched TDS data on request. 6. Processing Notes Field experience with cardanol diglycidyl ether YLD-9014A reduces to a short list: Add the diluent to the resin first and homogenize before dosing the hardener; adding it after the amine invites local stoichiometry errors. Cold warehouses push viscosity toward the top of the 1000-3000 mPa·s window. In practice, check viscosity at room temperature, not straight off a winter pallet. The reddish brown tone (Color max. 18) shows through light-colored topcoats. When color is critical, a paler grade such as YLD-9016 (max. 12) is the better fit. Batches differ inside the published ranges. If the hardener ratio is calculated tight, feed incoming COA values into the phr math rather than last year's averages. Amine adducts prepared on a difunctional ether usually gel a little differently from those on monofunctional ethers; run a gel-time check before locking pot life. Store cool, dry, and out of direct sunlight, and keep drums sealed because glycidyl ethers pick up moisture slowly in humid climates. 7. Applications YLD-9014A earns its place where viscosity, toughness, and water resistance have to move together. Typical uses reported for the grade: Application Role of YLD-9014A Structural and general adhesives Raises bond strength and flexibility while limiting loss of mechanical strength High-solids coatings Viscosity reduction with lower VOC emissions Solvent-free (2K) systems Reactive diluent that co-cures instead of evaporating Composites and FRP Toughening agent and impregnation aid in winding and pultrusion lines Modified curing agents Building block for amine adducts The same logic runs across the families documented in epoxy resin adhesives and epoxy resin coatings: wherever a brittle network fails in wet or impact service, the cardanol backbone is worth a trial. For structural work, see epoxy resin composites. 8. Frequently Asked Questions What is cardanol diglycidyl ether YLD-9014A used for? YLD-9014A works as a reactive diluent and toughening agent in epoxy adhesives, high-solids and solvent-free coatings, composites, and amine adduct curing agents. It cuts blend viscosity while adding flexibility, water resistance, and adhesion strength. What is the CAS number of YLD-9014A? CAS No. 68390-54-5 belongs to cardanol diglycidyl ether YLD-9014A. The sibling grades YLD-9014 and YLD-9016 share the same CAS, since they carry the same cardanol diglycidyl ether chemistry but different EEW and viscosity windows. How is YLD-9014A different from YLD-9014? Both are difunctional cardanol diglycidyl ethers in the same 1000-3000 mPa·s band. The difference is EEW: YLD-9014A runs 200-270 g/eq against 290-350 g/eq for YLD-9014. The lower value means more epoxy groups per kilogram, so YLD-9014A cures more reactively and builds a tighter network. Choose the standard grade when you want the maximum flexibility and the lowest reactivity, and YLD-9014A when reactivity or hardness retention matters more. How much YLD-9014A should I add to an epoxy formulation? Most systems start between 5 and 15 phr. The right level depends on how much flexibility you can trade against Tg: above roughly 20 phr, hardness and heat resistance drop noticeably. Verify the final dosage against your own cure schedule. Can YLD-9014A be used as a standalone resin? Yes. YLD-9014A can run as a modifier in conventional epoxy systems or as the standalone resin when flexibility is the priority. Standalone use is not the right choice for neat casting that needs high rigidity, because the cardanol backbone keeps the cured part flexible by design. How should YLD-9014A be stored and how long does it last? Store in a cool, dry place away from direct sunlight with drums sealed. Shelf life is 12 months from the date of manufacture in the original packing at ambient temperature. All safety handling details are provided in the MSDS. 9. Packaging, Storage and Safety Packaging is a 200 kg drum. Shelf life is 12 months from the date of manufacture in the original sealed packing at ambient temperatures. Store in a cool and dry place and avoid direct sunlight. Keep containers closed when not in use, because most glycidyl ethers slowly absorb moisture in humid storage. All safety information is provided in the Material Safety Data Sheet that accompanies every shipment and is available on request. For samples, current batch COAs, or help matching a grade to a viscosity target, contact the product team on the YLD-9014A product page or browse the full range on the diluent and glycidyl ether category page.
    Read More
  • Cardanol Diglycidyl Ether YLD-9014: Toughening Epoxy Diluent
    Cardanol Diglycidyl Ether YLD-9014: Toughening Epoxy Diluent
    Oct 03, 2026
    Cardanol diglycidyl ether YLD-9014 is a bio-based difunctional epoxy reactive diluent with EEW 290-350 g/eq and a viscosity of 1000-3000 mPa·s at 25°C. The cashew-oil derived molecule cuts viscosity in high-solids coatings and adhesives while adding toughness, moisture resistance, and bond strength. Product Code: YLD-9014 CAS No.: 68390-54-5 Product Category: Diluent & Glycidyl Ether 1. Product Information The grade ships as a reddish brown liquid in 200 kg drums, with Gardner color max. 18 and water content max. 0.2%. The table below collects the published product data in one place. Item Information Product Code Cardanol Diglycidyl Ether YLD-9014 Chemical Name Cardanol diglycidyl ether, cashew oil modified difunctional glycidyl ether CAS No. 68390-54-5 Appearance Reddish brown liquid Color, G Max. 18 EEW, g/eq 290-350 Viscosity (25°C) 1000-3000 mPa·s Water content Max. 0.2% Packaging 200 kg drum Shelf life 12 months from date of manufacture, original sealed packing 2. Product Description: How YLD-9014 Toughens Epoxy Systems Chemically, cardanol diglycidyl ether YLD-9014 is a cashew oil modified difunctional glycidyl ether. Two glycidyl groups sit on a long-alkyl cardanol backbone, so the molecule co-reacts into the cured network instead of staying in it as a free plasticizer. That is the difference between a reactive diluent and a solvent. The long hydrophobic alkyl chain does three jobs at once. It drops the blend viscosity so high-solids and solvent-free systems can be pumped, mixed, and wetted out. It internal-plasticizes the network, which is where the flexibility and impact resistance come from. And it repels water, so cured films keep their properties in wet service better than many petrochemical-diluent systems. One more practical point. Cardanol-based diluents tolerate imperfect surfaces: when the substrate carries traces of moisture or light oil, YLD-9014-based formulations hold adhesion where a brittle neat resin would peel. Surface preparation still matters, but the margin is wider. Compatibility with conventional epoxy systems is built in, and YLD-9014 can also be used as a standalone resin when flexibility outweighs hardness. It is derived from botanical extracts, a renewable and non-toxic raw material base, which helps with VOC and labeling discussions in export markets. 3. YLD-9014 vs Alternative Reactive Diluents The main alternatives are the low-viscosity monofunctional ethers and the other cardanol grades in the same family. The table below compares published specifications side by side. Property YLD-9014 YLD-9014A YLD-9016 YLD-9006 BGE YLD-9004A Functionality Difunctional Difunctional Bifunctional Monofunctional Monofunctional EEW, g/eq 290-350 200-270 250-330 355-500 147-157 Viscosity (25°C), mPa·s 1000-3000 1000-3000 60-150 30-50 Max. 2 Raw material base Cashew oil, bio-based Cashew oil, bio-based Cashew oil, bio-based Cashew oil, bio-based Petrochemical Typical role Toughener-diluent for adhesives and composites Flexible-rigid balance in coatings Low-viscosity AGE/BGE alternative General diluent, low odor Fast viscosity cut Every reactive diluent is a trade-off: flexibility and water resistance go up, while Tg and hardness come down. If your formulation needs film hardness more than flexibility, cardanol diglycidyl ether YLD-9014A is the closer match; it balances flexible and rigid segments and holds impact resistance without going soft. If the job is a deep viscosity cut instead, the numbers above say it plainly. Cardanol diglycidyl ether YLD-9016 sits at 60-150 mPa·s, and cardanol glycidyl ethers YLD-9006 at 30-50 mPa·s. YLD-9014, at 1000-3000 mPa·s, is not the tool for that. Against BGE, the honest comparison is odor and property retention. A butyl glycidyl ether BGE YLD-9004 blend thins faster and costs less per liter, but the cardanol grades are widely positioned as non-toxic alternatives to AGE and BGE, with less impact on cured thermal properties and no irritating odor. In export projects with RoHS-style halogen-free and low-odor requirements, that usually decides the argument. 4. Typical Technical Information of Cardanol Diglycidyl Ether YLD-9014 Cardanol diglycidyl ether YLD-9014 is specified by five published parameters: appearance, Gardner color, epoxy equivalent weight, viscosity, and water content. The values below are the published specification ranges. Item Specification Appearance Reddish brown liquid Color, G Max. 18 EEW, g/eq 290-350 Viscosity (25°C), mPa·s 1000-3000 Water, % Max. 0.2 Treat these as specification ranges, not batch certificates. Confirm the current batch against the TDS, MSDS, and COA before you release a formulation to production, and re-check EEW on incoming material if your hardener ratio is calculated tight. 5. Formulation and Selection Guidance YLD-9014 carries epoxy groups of its own, so it consumes hardener like any other epoxide. The stoichiometry is straightforward. blend EEW = 1 / (w1/EEW1 + w2/EEW2), then hardener phr = 100 × AHEW / blend EEW. Worked example. Take 90 parts of a bisphenol F epoxy resin (EEW 170, such as the site's bisphenol F epoxy resin grade) plus 10 parts YLD-9014 at its EEW midpoint of 320 g/eq. Blend EEW = 1 / (90/170 + 10/320) = 178 g/eq. With a dicyandiamide-derivative hardener at AHEW 60, demand is 100 × 60 / 178 = 33.7 phr, versus 35.3 phr for the neat resin. The exact number depends on your accelerator package and cure schedule; treat 33.7 phr as a starting point, not a specification. Viscosity responds fast but not dramatically, because YLD-9014 itself sits at 1000-3000 mPa·s. A log-rule estimate for 10 parts YLD-9014 (taken at 2000 mPa·s) into 90 parts of a 15,000 mPa·s resin gives roughly 12,300 mPa·s, an 18% cut. If your line needs to get below 1000 mPa·s, YLD-9016 is the grade built for that, not YLD-9014. As a starting window, most formulators run YLD-9014 at 5-15 phr against standard liquid epoxy resins. Above roughly 20 phr the network softens noticeably; check the heat-deflection numbers on your own system before committing. We can supply grade-matched TDS data on request. 6. Processing Notes Field experience with cardanol diglycidyl ether YLD-9014 boils down to a short list: Add the diluent to the resin first and homogenize before dosing the hardener; adding it to the mix after the amine invites local stoichiometry errors. Cold warehouses push viscosity toward the top of the 1000-3000 mPa·s window. In practice, check viscosity at room temperature, not straight off a winter pallet. Amine adducts prepared on YLD-9014 usually cure a little slower than adducts on monofunctional ethers; plan pot life and post-cure accordingly. The reddish brown tone (Color max. 18) will show through light-colored topcoats. When color is critical, YLD-9016 (max. 12) is the paler choice. Batches differ inside the published ranges. If your hardener ratio is calculated tight, run incoming COA values into the phr math rather than last year's averages. Storage is cool, dry, and out of direct sunlight; keep drums sealed because glycidyl ethers pick up moisture slowly in humid climates. 7. Applications YLD-9014 earns its place where viscosity, toughness, and water resistance must move in the same direction. Typical uses reported for the grade: Application Role of YLD-9014 Structural and general adhesives Raises bond strength and flexibility while limiting loss of mechanical strength High-solids coatings Viscosity reduction with lower VOC emissions Solvent-free (2K) systems Reactive diluent that co-cures instead of evaporating Composites and FRP Toughening agent and impregnation aid in winding and pultrusion lines Modified curing agents Building block for amine adducts The same logic extends across the product families documented in epoxy resin adhesives and epoxy resin coatings: wherever a brittle network fails in wet or impact service, the cardanol backbone is worth a trial. For structural composites, see epoxy resin composites. 8. Frequently Asked Questions What is cardanol diglycidyl ether YLD-9014 used for? YLD-9014 works as a reactive diluent and toughening agent in epoxy adhesives, high-solids and solvent-free coatings, composites, and amine adduct curing agents. It cuts blend viscosity while adding flexibility, water resistance, and adhesion strength. What is the CAS number of YLD-9014? Cardanol diglycidyl ether YLD-9014 has CAS No. 68390-54-5. The same CAS applies to the sibling grades YLD-9014A and YLD-9016, which share the cardanol diglycidyl ether chemistry but differ in EEW and viscosity windows. How much YLD-9014 should I add to an epoxy formulation? Most systems start between 5 and 15 phr. The right level depends on how much flexibility you can afford to trade against Tg: above roughly 20 phr, hardness and heat resistance drop noticeably. Verify the final dosage with your own cure schedule. What is the difference between YLD-9014 and YLD-9014A? Both are difunctional cardanol diglycidyl ethers at 1000-3000 mPa·s. YLD-9014A has a lower EEW window (200-270 g/eq versus 290-350 g/eq) and combines flexible and rigid segments, so it holds film hardness and impact resistance better; YLD-9014 is the tougher, more flexible choice. Does YLD-9014 slow down the epoxy cure? The glycidyl groups are reactive, so the network cures normally, but amine adducts built on YLD-9014 usually set a little slower than those on monofunctional ethers. If cycle time is tight, run a DSC or gel-time check on your own hardener package before locking the recipe. How should YLD-9014 be stored and how long does it last? Store in a cool, dry place away from direct sunlight, drums sealed. Shelf life is 12 months from the date of manufacture in the original packing at ambient temperature. All safety handling details are provided in the MSDS. 9. Packaging, Storage and Safety Packaging is a 200 kg drum. Shelf life is 12 months from the date of manufacture in the original sealed packing at ambient temperatures. Store in a cool and dry place and avoid direct sunlight. Keep containers closed when not in use; like most glycidyl ethers, the material slowly absorbs moisture in humid storage. All safety information is provided in the Material Safety Data Sheet, which accompanies every shipment and is available on request. For samples, current batch COAs, or help matching a grade to your viscosity target, contact the product team on the YLD-9014 product page or browse the full diluent range on the diluent and glycidyl ether category page.
    Read More

leave a message

leave a message
If you are interested in our products and want to know more details,please leave a message here,we will reply you as soon as we can.
submit

home

products

WhatsApp

Contact Us